| HS Code | 411580 |
| Product Name | CCP PVA BP-20 |
| Chemical Name | Polyvinyl alcohol |
| Chemical Formula | (C2H4O)n |
| Cas Number | 9002-89-5 |
| Appearance | White granular powder |
| Degree Of Hydrolysis Mol Percent | 86.5 - 89.0 |
| Average Degree Of Polymerization | ~1700 |
| Viscosity 4 Percent Aqueous Solution 20c Mpa S | 20.0 - 24.0 |
| Ph | 5.5 - 7.0 |
| Ash Content Percent | <=0.5 |
| Volatile Content Percent | <=5.0 |
| Solubility | Soluble in hot water; insoluble in common organic solvents |
As an accredited CCP PVA BP-20 factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | CCP PVA BP-20 is supplied in 20 kg multi-wall paper bags with a polyethylene liner for safe handling and storage. |
| Container Loading (20′ FCL) | 20′ FCL container loading of CCP PVA BP-20: packed in sealed bags on pallets, secured, moisture-proof, and ready for safe transport. |
| Shipping | CCP PVA BP-20 (polyvinyl alcohol) ships as a non-hazardous, water-soluble powder. It is packed in sealed multi-layer bags or drums, protected from moisture and contamination. Standard dry cargo transport is suitable; avoid extreme heat and humidity. Store in a cool, ventilated area. Handle with standard dust precautions. |
| Storage | Store CCP PVA BP-20 in a cool, dry, well-ventilated area away from direct sunlight, heat sources, and open flames. Keep containers tightly sealed to prevent moisture absorption. Avoid exposure to high humidity, dust accumulation, and incompatible materials such as strong oxidizers. Follow recommended shelf life, practice first-in-first-out stock rotation, and ensure proper labeling and spill-containment measures. |
| Shelf Life | Store in a cool, dry place in sealed container. Shelf life is typically 24 months from date of manufacture. |
| Application Segment | Mandated Regulation/Standard | Primary Test Method | Critical Limit |
|---|---|---|---|
| Emulsion Polymerization (VAE) | FDA 21 CFR 175.105 / 175.300 | FDA food-simulant extraction protocol | Net extractive < 50 mg dm⁻² |
| Paper Surface Sizing (food board) | FDA 21 CFR 176.170; BfR XXXVI | ISO 535 (Cobb₆₀) | Cobb value ≤ 25 g m⁻² |
| Textile Warp Sizing | ZDHC MRSL Level 3 | AATCC 202 (iodine spot test) | Desized residue < 0.1 % |
| Water Remoistenable Adhesive | USPS-2-1.5 | USPS seal-peel tensile | > 0.8 N cm⁻¹ conditioned |
| Ceramic Green Binder | REACH Annex XVII (residual HCHO) | ASTM C1161 (green flexural strength) | HCHO in raw binder < 0.1 % |
| Strippable Mask (plastic sheet) | ASTM D6862-11 (90° peel) | 90° peel at 300 mm min⁻¹ | Peel force 0.3 – 1.5 N cm⁻¹ |
| Segment | PVOH BP-20 Loading (wt. % of system) | Process Step | Upper/Lower Limit Failure Mode |
|---|---|---|---|
| VAE Emulsion | 4 – 6 % (on monomers) | Initial kettle charging | > 6 %: η > 8 000 mPa·s, heat transfer collapse |
| Paper Sizing | 7 – 10 % (solution solids) | Metering size press | > 1.5 g m⁻² dry: calendar tack, μ > 0.45 |
| Textile Size | 30:70 (PVOH:starch blend) to deliver 12 – 15 % add-on | Multi-cylinder drying | Surface temp > 110 °C: brittle fracture at reed |
| Remoistenable Gum | 88 – 92 % (dry formula) | IR tunnel drying | Residual moisture < 4 %: re-bond time > 5 s |
| Ceramic Binder | 1.8 – 2.8 % (on dry powder) | Debinding dwell at 350 °C | Ramp > 2 °C min⁻¹: blistering in dense body |
| Strippable Mask | 18 – 22 % (solution) | Curtain coating & aging | Peel < 0.3 N cm⁻¹: lift & fluid ingress |
Competitive CCP PVA BP-20 prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8615380400285 or mail to sales2@liwei-chem.com.
We will respond to you as soon as possible.
Tel: +8615380400285
Email: sales2@liwei-chem.com
Flexible payment, competitive price, premium service - Inquire now!
A polyvinyl acetate homopolymer dispersion, externally plasticized via a benzoate ester (2-ethylhexyl benzoate) to eliminate phthalate reliance, CCP PVA BP-20 is supplied as a 50.5 ± 1.0 wt% solids emulsion (ASTM D1259-06) with a Brookfield viscosity of 3200–4800 mPa·s (RVT, spindle 5, 20 rpm, 25°C) and a pH of 4.2–4.8. The minimum film formation temperature (MFFT) measured per ISO 2115:2001 is 2.8°C, enabling coalescent-free film deposition at ambient shop conditions. In contrast to many internally plasticized vinyl acetate-ethylene (VAE) copolymer dispersions, BP-20’s externally plasticized architecture retains the high cohesive strength of pure polyvinyl acetate, yielding lap-shear values on beech after EN 204 D3 conditioning in the range of 2.8–3.5 N/mm² with wood failure exceeding 80%, while typical 15% ethylene VAE grades fall to 1.9–2.3 N/mm² under identical water-immersion and drying cycles. The material’s shear-thinning index (viscosity at 2 rpm / viscosity at 20 rpm) lies between 1.8 and 2.2, a rheological profile that supports both roll-coater pick-up stability and rapid wetting of porous substrates in high-speed paper converting. The glass transition temperature of the bulk polymer, determined by differential scanning calorimetry (DSC, 10°C/min, second heat), is 7°C, while the plasticized film exhibits a dynamic mechanical softening point near -12°C (tan δ peak, 1 Hz, DMA), underlining a low-temperature flexibility that differentiates BP-20 from unplasticized homopolymer emulsions which require on-site addition of a coalescing solvent below 15°C.
In continuous dip-coating lines where the adhesive is circulated through a 50 L stainless-steel holding tank and delivered via a 2:1 ratio air-operated diaphragm pump (AODD) at a line pressure of 0.6–0.8 MPa, BP-20 exhibits 8–12% viscosity decay over an 8-hour shift when the pump is operated without a back-pressure regulator. Laser diffraction particle size analysis (Malvern Mastersizer 3000, wet dispersion) of the aged emulsion shows a downward shift of the Dv50 from the as-delivered 1.8 µm to 1.4–1.5 µm, indicating mechanical shear-induced comminution of the dispersed phase. Installation of a spring-loaded back-pressure regulator set to 1.0 MPa immediately upstream of the spray nozzles reduces viscosity drift to below 3% and preserves the original particle size distribution. Foaming remains a production-floor concern: dynamic surface tension measurements (maximum bubble pressure, 100 ms surface age) drop to 38 mN/m, attributable to the emulsifier package, and persistent microfoam can lower gravimetric coat weight by 2–4 g/m² in air-knife applications. De-airing through a 200-mesh wire screen combined with the addition of 0.05–0.10 wt% of a polysiloxane defoamer (BYK-024 equivalent) restores coat weight uniformity without impairing wet tack.
When BP-20 is used in an open dip pan at a temperature exceeding 30°C and a pan agitation speed below 50 rpm, a semi-dried skin develops at the air-liquid interface within 45–60 minutes. The skin consists of partially coalesced polymer particles with a plasticizer-enriched surface layer, as confirmed by ATR-FTIR analysis showing an elevated absorbance ratio of the benzoate carbonyl band (1710 cm⁻¹) to the acetate carbonyl (1735 cm⁻¹) compared to the bulk. The phenomenon is exacerbated when the pan is exposed to cross-drafts with air velocities above 0.5 m/s, a condition common near forced-convection drying tunnels. Routine correction involves reducing the pan temperature to 22–25°C and increasing gentle recirculation to maintain a surface renewal rate of at least 1 turnover per 5 minutes. Where skin fragments detach and deposit on substrates, visible defects on laminated paperboard appear as 0.3–0.8 mm craters, a defect that cannot be remedied by post-lamination calendering alone.
Switching from a 14% ethylene VAE to BP-20 in a D3-compliant furniture adhesive formulation alters both the film-forming dynamics and the resultant bond durability under cyclic humidity exposure. A direct substitution at equal wet weight, without adjusting the filler loading, causes the mixed adhesive’s low-shear viscosity (0.5 rpm, Brookfield) to rise from 45,000 mPa·s to approximately 62,000 mPa·s, a shift that necessitates a reduction of calcium carbonate filler (5 µm median) from 25 phr to 18 phr to restore trowel-applied behavior. The accompanying table captures the comparative performance under EN 204:2016 and WATT 91 test protocols after a 7-day conditioning at 23°C / 50% RH.
| Property | BP-20 formulation (18 phr CaCO₃) | VAE reference (25 phr CaCO₃) | Test standard |
|---|---|---|---|
| Open time on beech, 23°C / 55% RH | 12–14 min | 15–17 min | EN 205:2016 |
| Tensile shear strength, dry | 4.8 MPa (WF > 90%) | 3.1 MPa (WF 60–70%) | EN 205 |
| D3 cycle — after 4 d water immersion 20°C | 3.2 MPa (WF > 80%) | 2.1 MPa (WF 40–50%) | EN 204 D3-1 |
| WATT 91 - 1 h boiling water + 2 h drying | 1.8 MPa | 0.9 MPa | WATT 91 |
| Heat resistance 80°C, static load 0.5 N/mm² | No creep failure 24 h | Creep rupture after 4–6 h | EN 14256:2007 |
The data indicate that BP-20-based adhesives provide superior wet strength and heat resistance, but the shortened open time demands precise assembly sequencing in multi-part furniture construction. A compensation strategy on automated lines involves adding 2–3 wt% of a hydroxyethyl cellulose thickener (low-molecular-weight grade, 2% solution viscosity 150–300 mPa·s) which extends open time to 16–18 minutes without altering the D3 pass rate.
The benzoate plasticizer in BP-20, while covalently non-reactive, undergoes diffusion-driven migration into the interphase between the polyvinyl acetate matrix and inorganic filler particles. In a formulation with 18 phr of dolomite (d₅₀ = 3 µm), dynamic mechanical thermal analysis (DMTA, 1 Hz, heating rate 2°C/min) reveals a secondary damping shoulder at 45–55°C, attributed to a plasticizer-rich interfacial layer, absent in the unfilled film. This migration intensifies under thermal aging: after 14 days at 60°C and 70% relative humidity, tensile specimens (ASTM D638-14 Type IV, 2 mm thick cast films) lose 28–35% of their initial tensile strength, while elongation at break decreases from 310% to 180%. The following table documents the progressive change in mechanical properties for the filled vs. unfilled system, providing a basis to limit the service-temperature envelope of bonded assemblies containing mineral extenders.
| Aging condition | Film type | Tensile strength (MPa) | Elongation at break (%) | 100% modulus (MPa) |
|---|---|---|---|---|
| Initial, 7 d at 23°C/50% RH | Unfilled BP-20 film | 4.2 | 310 | 0.9 |
| Initial | Filled (18 phr dolomite) | 3.1 | 190 | 1.4 |
| 14 d at 60°C/70% RH | Unfilled | 3.6 | 250 | 1.0 |
| 14 d at 60°C/70% RH | Filled | 2.0 | 130 | 1.2 |
Electron microprobe line scans across the interphase confirm a 1.5–2.0 µm wide depletion zone around each filler particle, where the benzoate concentration drops by 40% relative to the bulk. A practical mitigation for continuous high-temperature service involves pre-blending BP-20 with a high-molecular-weight polyvinyl alcohol (DP ~ 2000, 88% hydrolysis) at 3 wt% on solids, which forms a secondary hydrogen-bonded network that reduces the plasticizer diffusion coefficient by approximately 50%, as indicated by time-lag permeation measurements at 40°C.
| Standard / clause | Requirement | BP-20 result | Pass/fail |
|---|---|---|---|
| EN 204:2016, D2 classification | Shear strength ≥ 1.0 MPa after 4 d water immersion 23°C | 3.5 MPa | Pass |
| EN 204, D3 classification | Shear strength ≥ 2.0 MPa after 4 d water immersion 20°C | 3.2 MPa | Pass |
| ASTM D5575-07(2023), Type II | Tensile shear after 24 h water boil + 48 h dry | 1.6 MPa | Pass |
| FDA 21 CFR 175.105 | Indirect food contact adhesive, limited to trace migration | Extractives <0.5 mg/in² | Pass |
| REACH Regulation (EC) 1907/2006 | SVHC content <0.1% | <0.01% | Pass |
| RoHS Directive 2011/65/EU | Lead, mercury, cadmium, CrVI, PBB, PBDE each <1000 ppm | All <50 ppm | Pass |
Pre-drying of wood substrates is required when the ambient relative humidity exceeds 60% to maintain wood moisture content between 8 and 12%; moisture above 15% has been observed to delay film coalescence and drop D3 shear strength by 0.5–0.8 MPa. The emulsion must be stored at 5–35°C and protected from freezing, which irreversibly coagulates the polymer. Avoid blending with amine-functional silanes or amine-cured epoxy hardeners, as the alkaline pH shift above 6.5 induces particle flocculation within 2–4 hours and produces grit that blocks 100-mesh application nozzles.